Model : TERELENA TWR-II-200 - Caustic Soda Fabric Mercerizing Weight
Reduction Machine
Special Features & Technical Data :
The TERELENA treatment and process are applicable to both texturised and staple polyester, they permanently modify the physical character of the fiber by creating many micro-cavities which greatly increase the surface area and consequently the surface tension.
TERELENA is more than a simple process for improving drape, soft hand and achieving a silk like depth of lustre. TERELENA treatment by extracting polyester from the surface of the fiber to form micro cavities, causes a reduction of fabric weight. The purpose of our TERELENA UNIT is to add quality and value to polyester fabrics. To achieve comfort, soft hand, drape, transpiration, soil- release effect, electrostatic conductivity, moisture absorbency, elimination of synthetic
fiberglass complete uniformity and repeatability with auto system, simplicity of operation full control of the parameters which influence the process (with PLC machines only). Saving of dyestuff in subsequent processing, increased penetration of printing paste, improves response to sueding or raising.
The technician operating our system can set the parameter values which provide the complete uniformity, reproductibility of the terelena process namely a bath concentration, absorption of alkaline solution, reaction temperature, reaction time and fabric characteristics.
Fabric Loading Capacity: Kg 160-200
LIQUORE CAPACITY
Min : Liter:600-800
Max: Liter: 1200-1600
Steam Consumption(Min-Max): Kg/Batch 32-85
Cooling Water Consumption (Min-Max): Liter/Batch 400-1065
Electric Connected Load: Kw/HP: 9.32/12.5
Recovery Tank Capacity: Liters 1800
Max Operating Temp.: °C 98
Approx. Fabric Speed: Meters/Min 100-250
Heating Rate (70°C-98°C) (At 6 Bar Saturated Steam): Min 10
Cooling Rate (98°C-50°C) (Water Pressure At 1 Bar): Min 15
Cooling Method/Heating Method: Indirect
Floor Space Required
Length: mm 5450
Vessel Width (A): mm 1050
Total Width (B): mm 3050
Height: mm 4290
|